Broad distribution relative molecular weight HPAM (“B-HPAM” for short) was produced by mixing with three kinds of<br>different HPAM at different weight ratios, whose viscosity-average molecular weight were 19×106, 25×106, 35×106,<br>respectively. During the chemical flooding stage, the small flow resistance in high permeability formation led the HPAM<br>solution to flow through easily. Firstly the larger polymer clews absorbed in the larger pore throat and then the smaller clews<br>absorbed in the smaller pore throat. Enlarged the swept volume and enhanced oil recovery. Therefore, it was a promising<br>profile control method.

Loading

Article metrics loading...

/content/papers/10.3997/2214-4609-pdb.280.iptc14352_noPW
2012-02-07
2024-03-19
Loading full text...

Full text loading...

http://instance.metastore.ingenta.com/content/papers/10.3997/2214-4609-pdb.280.iptc14352_noPW
Loading
This is a required field
Please enter a valid email address
Approval was a Success
Invalid data
An Error Occurred
Approval was partially successful, following selected items could not be processed due to error